One of the acids, only concentrated nitric or sulfuric acid or aqua regia (a combination of nitric and hydrochloric acids) assault germanium appreciably. Despite the fact that aqueous caustic methods create tiny effect on it, germanium dissolves rapidly in molten sodium hydroxide or potassium hydroxide, therefore forming the respective germanates.I